Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 5.20 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO 180
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Izod Impact, Notched (ISO) 5.20 kJ/m²

@Temperature -40.0 °C
2.47 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Phillips Sumika Marlex® CHP-275 Thermoplastic Polyolefin  (discontinued **)
Engineered Thermoplastic Polyolefin.Applications: Automotive Head and Side Impact TrimConditioning after Molding: 48 hr at 23°C, 48 hr at 90°CNominal Shrinkage: 0.7-0.9%, 0.8-1.1%Drying conditions..
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO 180
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Izod Impact, Notched (ISO) 5.20 - 35.0 kJ/m²
2.47 - 16.7 ft-lb/in²
Average value: 10.8 kJ/m² Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO 180/1A
Lucite International Diakon® TD542 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry)
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6.
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® NBX-0025 NF2001 PA66 (Dry)
Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6.
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Ultramid 1000-11 NF2001 is a general purpose nylon 6/6.
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® 1000-2 NF2001 PA66 (Dry)
Ultramid 1000-2 NF2001 is a general purpose PA6/6.
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO Test
BASF Ultramid® 1003-2 NF2002 PA66 (Dry)
Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6.