Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
Type A; ISO 180:2000
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized
HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
PTS PBT-101G0 PBT Resin
Typical Applications: Appliance partsInformation provided by PTS LLC.
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
Sample Type A; ISO 180:2000
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-MFC-G0 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
BLUESTAR 101G0 PBT
Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G0 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G0 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 5.40 kJ/m²

@Temperature -40.0 °C
2.57 ft-lb/in²

@Temperature -40.0 °F
ISO Test
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry)
Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance ..
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Star L PA66 15Y D61 PA66, Carbon Filled, Injection Molded
Star L PA66 15Y D61 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.