Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.70 kJ/m² @Temperature -40.0 °C |
3.66 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Izod Impact, Notched (ISO) | 7.70 kJ/m² | 3.66 ft-lb/in² | ISO 180 |
BASF Ultramid® 66 H2 G/25-V0KB1 NAT 0046 PA66 (Dry) Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 7.70 kJ/m² @Temperature 23.0 °C |
3.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly.. |