Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/A |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ASTM D256 |
JPJ Technologies PP C120 PP Copolymer Injection Molding Information provided by JPJ Technologies |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | Notch A; ISO 180 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | Notch A; ISO 180 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GFT1525-BK 15% Glass Fiber Reinforced, Impact Modified Nylon 6 Description: Glass Fiber Reinforced, Impact Modified Nylon 6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/1A |
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene POLYSTYRENE IMPACT 6540 is an easy flowing, high impact polystyrene with a good balance of mechanical and thermal properties. This resin combines physical properties such as the flow necessary for .. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180 |
Polyram RamTough RZ321G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ASTM D256 |
Total PSI 3351 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 3351 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional st.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180 |
Polyram RamTough RZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO Test |
BASF Petra® 7030 GY6128 30% Glass Filled PET Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO Test |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO Test |
BASF Ultramid® A3EG7 BK00564 35% Glass Filled PA66 (Dry) Ultramid A3EG6 BK00564 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO Test |
BASF Ultramid® A3EG7 BK23189 35% Glass Filled PA66 (Dry) Ultramid A3EG6 BK23189 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 9.50 - 17.9 kJ/m² | 4.52 - 8.52 ft-lb/in² | Average value: 12.8 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
Izod Impact, Notched (ISO) | 9.50 - 13.0 kJ/m² | 4.52 - 6.19 ft-lb/in² | Average value: 10.7 kJ/m² Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/A |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |