Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 631 kg | 1390 lb (mass) | Init. Seiz. Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® M30 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Four Ball Extreme Pressure, Weld Load | 631 kg | 1390 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® M30 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Four Ball Extreme Pressure, Weld Load | 631 kg | 1390 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® W500 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |