Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -20.0 °C |
6.19 ft-lb/in² @Temperature -4.00 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical HF-350 ABS, High Flow, High Impact Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 136F3Q32 Nylon 6, 15% Glass Fiber SAXAMID 136F3Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 15% glass fibers with very high impact properties. Beside the high impact strength at low temperatures .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram PlusTek PA310G8BK10 Nylon 6.6 for injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% Glass fiber reinforced Nylon 6.6 for injection molding applications. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 179/1eA |
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |