Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR40 NL100 PBT, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR25 NL PA 6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecopet® PT70 GR45 NL100 PR PET, 45% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry) Description: Ultramid 66 H2 G/35-V0KB NAT0046 is a 35% glass reinforced, heat stabilized injection molding grade. It is a V-0 self-extinguishing grade, with phosphorous. It offers good flowability a.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |