Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1A |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 0.000 °C |
9.52 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
ISO 180/A |
Styrolution Novodur® 530 ABS Novodur 530 is an extrusion grade optimized for sheet applications. It has high impact properties, high modulus and good thermoforming.Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR45 NL HS PA6, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL IH PA 6.6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |