Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | >= 1010 x 10-8 mm³/N-M | >= 500 x 10-10 in³-min/ft-lb-hr | QTM55010 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 1010 x 10-8 mm³/N-M | 500 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
K (wear) Factor | 1010 x 10-8 mm³/N-M | 503 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |