Polymer Property : K (wear) Factor = 20.1 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
QTM55010
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66
LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66
LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific)
LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA
LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
K=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours).
A. Schulman ComAlloy Lubrilon® 605 Nylon 6/6, PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
K (wear) Factor 20.1 x 10-8 mm³/N-M
10.0 x 10-10 in³-min/ft-lb-hr
With post-machine cure cycle; QTM 55010
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet)