Mechanical Properties Metric English Comments
K (wear) Factor 66.5 x 10-8 mm³/N-M
33.0 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
K (wear) Factor 66.5 x 10-8 mm³/N-M
33.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific)
LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 66.5 x 10-8 mm³/N-M
33.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched
LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
K (wear) Factor 66.5 x 10-8 mm³/N-M
33.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East)
LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 66.5 x 10-8 mm³/N-M
33.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific)
LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.