Polymer Property : K (wear) Factor = 78.6 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 78.6 x 10-8 mm³/N-M
39.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear (Asia Pacific)
LNP* STAT-KON* OEP32 is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive.
K (wear) Factor 78.6 x 10-8 mm³/N-M
39.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear
LNP STAT-KON* OEP32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.