Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 112000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 770 MPa

@Strain 1.00 %
112000 psi

@Strain 1.00 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4313 Martensitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 774 MPa

@Treatment Temp. 427 °C,
Time 1.44e+7 sec
112000 psi

@Treatment Temp. 801 °F,
Time 4000 hour
0.2%. Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 772 MPa

@Temperature 93.3 °C
112000 psi

@Temperature 200 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel
Copyright © lookpolymers.com All Rights Reserved