Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 115 MPa @Strain 0.200 %, Temperature 400 °C |
16700 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 115 MPa @Strain 0.200 %, Temperature 400 °C |
16700 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 115 MPa @Strain 0.200 %, Thickness 150 - 500 mm |
16700 psi @Strain 0.200 %, Thickness 5.91 - 19.7 in |
Typical Strength |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | 115 MPa @Strain 0.200 %, Thickness 500 - 600 mm |
16700 psi @Strain 0.200 %, Thickness 19.7 - 23.6 in |
Typical Strength |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | 115 MPa @Strain 0.200 %, Thickness 150 - 500 mm |
16700 psi @Strain 0.200 %, Thickness 5.91 - 19.7 in |
Typical Strength |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 6.30 - 12.5 mm |
>= 16700 psi @Strain 0.200 %, Thickness 0.248 - 0.492 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 50.0 - 80.0 mm |
>= 16700 psi @Strain 0.200 %, Thickness 1.97 - 3.15 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 8.00 - 12.5 mm |
>= 16700 psi @Strain 0.200 %, Thickness 0.315 - 0.492 in |
Tempers O/H111; Standard EN 485-2 |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 12.5 - 50.0 mm |
>= 16700 psi @Strain 0.200 %, Thickness 0.492 - 1.97 in |
Tempers O/H111; Standard EN 485-2 |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 50.0 - 80.0 mm |
>= 16700 psi @Strain 0.200 %, Thickness 1.97 - 3.15 in |
Tempers O/H111; Standard EN 485-2 |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | 115 MPa @Strain 10.0 % |
16600 psi @Strain 10.0 % |
ASTM D95 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 6.00 - 12.5 mm |
>= 16700 psi @Strain 0.200 %, Thickness 0.236 - 0.492 in |
Temper H111; Standard EN 485-2 |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 12.5 - 50.0 mm |
>= 16700 psi @Strain 0.200 %, Thickness 0.492 - 1.97 in |
Temper H111; Standard EN 485-2 |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Tensile Strength, Yield | >= 115 MPa @Strain 0.200 %, Thickness 50.0 - 80.0 mm |
>= 16700 psi @Strain 0.200 %, Thickness 1.97 - 3.15 in |
Temper H111; Standard EN 485-2 |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |