Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 903 MPa @Strain 0.200 % |
131000 psi @Strain 0.200 % |
Longitudinal |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Tensile Strength, Yield | 903 MPa @Temperature -55.0 °C |
131000 psi @Temperature -67.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 903 MPa @Temperature 90.6 °C |
131000 psi @Temperature 195 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 900 - 1100 MPa @Strain 0.2 % |
131000 - 160000 psi @Strain 0.2 % |
as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Tensile Strength, Yield | 900 - 1170 MPa @Temperature 315 °C |
131000 - 170000 psi @Temperature 599 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Tensile Strength, Yield | 900 - 1170 MPa @Strain 0.200 %, Temperature 315 °C |
131000 - 170000 psi @Strain 0.200 %, Temperature 599 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Tensile Strength, Yield | 900 - 1170 MPa @Temperature 315 °C |
131000 - 170000 psi @Temperature 599 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |