Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1572 MPa @Temperature 23.0 °C |
228000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape Information provided by HexCel |