Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 110 MPa @Strain 0.200 %, Temperature 700 °C |
16000 psi @Strain 0.200 %, Temperature 1290 °F |
EN min. |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 110 MPa @Strain 0.200 %, Temperature 300 °C |
16000 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 % |
>= 16000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 110 MPa @Temperature -40.0 °C |
16000 psi @Temperature -40.0 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.57 mm |
16000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.57 mm |
16000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.10 - 1.60 mm, Temperature 982 °C |
16000 psi @Thickness 0.0433 - 0.0630 in, Temperature 1800 °F |
0.2% offset |
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 150 - 500 mm |
>= 16000 psi @Strain 0.200 %, Thickness 5.91 - 19.7 in |
Temper 03 |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 500 - 600 mm |
>= 16000 psi @Strain 0.200 %, Thickness 19.7 - 23.6 in |
Temper 03 |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 500 - 600 mm |
>= 16000 psi @Strain 0.200 %, Thickness 19.7 - 23.6 in |
Temper O3 |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 80.0 - 120 mm |
>= 16000 psi @Strain 0.200 %, Thickness 3.15 - 4.72 in |
Temper H111; Standard EN 485-2 |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |