Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1710 MPa @Temperature 71.0 °C |
248000 psi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel |