Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 147 MPa @Strain 1.00 %, Temperature 200 °C |
21300 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 0.200 %, Temperature 100 °C |
21300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 0.200 %, Temperature 100 °C |
21300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 1.00 %, Temperature 200 °C |
21300 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 0.200 %, Temperature 200 °C |
21300 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 0.200 %, Temperature 200 °C |
21300 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 147 MPa @Strain 0.200 %, Temperature 200 °C |
21300 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |