Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1779 MPa @Temperature 71.0 °C |
258000 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape Information provided by HexCel |