Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 352 MPa @Temperature 23.9 °C |
51000 psi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Tensile Strength, Yield | 352 MPa @Thickness 1.57 mm |
51100 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Tensile Strength, Yield | 352 MPa @Thickness 12.7 mm, Temperature 260 °C |
51100 psi @Thickness 0.500 in, Temperature 500 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 352 MPa @Temperature 25.0 °C |
51000 psi @Temperature 77.0 °F |
Open Hole Tensile, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 352 MPa @Strain 0.200 % |
51100 psi @Strain 0.200 % |
5% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |