Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.896 MPa @Temperature 93.0 °C |
565.1 psi @Temperature 199 °F |
Sandwich Flatwise Tension, Dry |