Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.481 MPa @Temperature 24.0 °C |
940.0 psi @Temperature 75.2 °F |
Flatwise TS |
Hexcel® HexPly® F155 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F155; Fiber: T300 Toho®Information provided by HexCel |