Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 65300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 450 MPa

@Strain 0.200 %
65300 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -80.0 °C
65300 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -80.0 °C
65300 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %,
Temperature 100 °C
65300 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4501 Duplex Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 450 MPa

@Strain 1.00 %,
Temperature -196 °C
65300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %
65300 psi

@Strain 0.200 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %,
Temperature 100 °C
65300 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %,
Thickness 1.45 mm
65300 psi

@Strain 0.200 %,
Thickness 0.0571 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %,
Thickness 240 - 305 mm
65300 psi

@Strain 0.200 %,
Thickness 9.45 - 12.0 in
Typical Strength
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %,
Thickness 160 - 180 mm
65300 psi

@Strain 0.200 %,
Thickness 6.30 - 7.09 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield 450 MPa

@Strain 0.200 %
65300 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..