Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 744 MPa @Strain 0.200 %, Thickness 3.20 mm |
108000 psi @Strain 0.200 %, Thickness 0.126 in |
Welded then age-hardened |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 744 MPa @Temperature 23.0 °C |
108000 psi @Temperature 73.4 °F |
T300; Fill Tension; (AMB) |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |