Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | at 2% offset; ASTM D882 |
ExxonMobil Escorene® LD 319.92 Film Resin
(discontinued **) Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 6.90 MPa | 1000 psi | ASTM D882 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Film Tensile Strength at Yield, MD | 6.90 MPa | 1000 psi | ASTM D882 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 6.90 MPa | 1000 psi | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Film Tensile Strength at Yield, MD | 6.90 MPa | 1000 psi | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Film Tensile Strength at Yield, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Film Tensile Strength at Yield, MD | 6.89 - 28.0 MPa | 1000 - 4060 psi | Average value: 11.1 MPa Grade Count:131 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |