Polymer Property : Film Tensile Strength at Yield, MD = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,..
Film Tensile Strength at Yield, MD 12.4 - 35.2 MPa
1800 - 5100 psi
Average value: 20.2 MPa Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
LyondellBasell Montell 12C01G2 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
LyondellBasell Montell 12C01G3 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: ..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
LyondellBasell Montell 12C01G5 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882, A
Total MDPE HL 323 Medium Density Polyethylene, Film Resin
Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin
Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
Dow LDPE 535I Low Density Polyethylene, Liner Grade
DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for..