Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D 1922 |
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922A |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922A |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922A |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922A |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM-D1922 |
Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FG31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blow film extrusion in blends with polyethylene. It has excellent mechanical propert.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM-D1922 |
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing .. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM-D1922 |
Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM-D1922 |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM-D1922 |
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These.. |
|||
Elmendorf Tear Strength MD | 100 g | 100 g | gF; ASTM D1922 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |