Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 332 g | 332 g | Method B; ASTM D1922 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |