Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
SABIC 6821N Linear Low Density Polyethylene for Blown Film
Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
SABIC HP0722N Low Density Polyethylene for Blown Film
Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti..
Elmendorf Tear Strength MD 350 g
350 g
Eastman E6838-997F Polyethylene  (discontinued **)
E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D 1922
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
LyondellBasell Petrothene® NA336149 Low Density Polyethylene
ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
LyondellBasell Petrothene® NA952000 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
LyondellBasell Petrothene® NA952094 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
LG Chemical SEETEC BF500 LDPE
Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength MD 350 g
350 g
Dow DOWLEX™ 2071 Linear Low Density Polyethylene
DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks..
Elmendorf Tear Strength MD 350 g
350 g
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regul..
Elmendorf Tear Strength MD 350 g
350 g
ASTM-D1922
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
LL4800N is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processi..
Elmendorf Tear Strength MD 350 g
350 g
ASTM-D1922
Braskem LL6801N LLDPE Blown Film Extrusion Polyethylene Copolymer
The LL6801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing ..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD..
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE  (discontinued **)
Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude..