Polymer Property : Elmendorf Tear Strength MD = 450 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 450 g
450 g
Eastman E6838-922F Polyethylene  (discontinued **)
E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat..
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b..
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
LG Chemical SEETEC BF315 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
Westlake Mxsten CV77512 Polyethylene Plastomer
Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex..
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
Westlake Mxsten CV77523 Polyethylene Plastomer
Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Elmendorf Tear Strength MD 450 g
450 g
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Elmendorf Tear Strength MD 450 g
450 g
ASTM D-1922
Bapolene® 152A Polyethylene Film Grade
Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Elmendorf Tear Strength MD 450 g
450 g
ASTM D-1922
Bapolene® 152B Polyethylene Film Grade
Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Elmendorf Tear Strength MD 450 g
450 g
ASTM D-1922
Bapolene® 152F Polyethylene Film Grade
Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin..
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
M. Holland Company MAGMA® LM124-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Elmendorf Tear Strength MD 450 g
450 g
ASTM D1922
M. Holland Company MAGMA® LM213-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.