Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | Orientation not specified; ASTM D882 |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | Orientation not specified; ASTM D882 |
DuPont™ Kapton® 50VN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | Orientation not specified; ASTM D882 |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 142 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 200 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 500 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 75 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 92 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Film Tensile Strength at Break, MD | 172 MPa | 24900 psi | ASTM D882 |
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |