Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 38.34 MPa | 5561 psi | ASTM D882 |
Dow DOWLEX™ 2038 Linear Low Density Polyethylene Linear Low Density PolyethyleneInformation provided by Dow |
|||
Film Tensile Strength at Break, MD | 38.34 MPa | 5561 psi | ASTM D882 |
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |