Polymer Property : Film Tensile Strength at Break, MD = 5500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 37.9 - 48.3 MPa
5500 - 7000 psi
ASTM D882
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 12C01G2 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 12C01G3 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: ..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 12C01G5 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 16502F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 16502F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
LyondellBasell Montell 16502F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Film Tensile Strength at Break, MD 37.9 MPa

@Thickness 0.0254 mm
5500 psi

@Thickness 0.00100 in
ASTM D882A
Total L425 HDPE Film
Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi..
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.