Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
DuPont™ Sclairfilm® MPP-1 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Film Tensile Strength at Break, MD | 82.7 - 138 MPa | 12000 - 20000 psi | ASTM D882 |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ 28UBW-ES OPP Film Product Description: A multi-layer, cavitaed, white OPP film with an enhanced sealant to allow sealing through contamination. This film has an exceptional barrier to gases, flavors, and moisture. It.. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
Dow Saran® 18L-WP White Plastic Barrier Film Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
Dow Saran® 28 Clear Plastic Barrier Film Saran™ 28 is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double wound rolls.Information prov.. |
|||
Film Tensile Strength at Break, MD | 82.7 MPa | 12000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These.. |