Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.72 MPa @Temperature 25.0 °C |
250 psi @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | at 100% secant; ASTM D638 |
Multibase Multi-Flex® A 5904 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | ASTM D-412 (Die C) |
Saint-Gobain Norcrylâ„¢ A2000 Solid Acrylic Bonding Tape Description: The Norcrylâ„¢ solid acrylic core has outstanding internal strength. Norcrylâ„¢ structural grade bonding power can reduce or replace conventional fasteners, rivets, liquid adhesiv.. |
|||
Tensile Strength, Yield | 1.72 MPa @Strain 300 % |
250 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1871R Thermoplastic Elastomer Notes: USP Class VI; ISO 10993; Clear Features: Good Stability Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 1.72 MPa @Strain 300 % |
250 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer Notes: General Purpose; CSA Approved; OpaqueInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | |
Master Bond Mastersil 800 One Component, Room Temperature Curing Silicone MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temp.. |
|||
Tensile Strength, Yield | 1.72 MPa @Strain 100 % |
250 psi @Strain 100 % |
Compound Property; Arlon SQA-TMS-008 |
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3050-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 1.72 MPa | 249 psi | cured 15 mins @ 150°C |
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | TM R050-36 |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | at 100% |
Resinlab® UR3010 Black Polyurethane Potting System Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | at 100% |
Resinlab® UR3010 Clear Polyurethane Potting System Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | at 100%; ASTM D412 |
G-2712 Styrene-based Biomedical Elastomer |
|||
Tensile Strength, Yield | >= 1.72 MPa | >= 250 psi | No units listed, assumed to be psi. |
Cos40 Cork/Neoprene Rubber Sheet Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot.. |
|||
Tensile Strength, Yield | 1.72 MPa | 250 psi | Transverse/Width |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.002" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |