Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM Data |
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Yield | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Tensile Strength, Yield | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010X PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized color.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
Polyram RamSter PF321G3 PBT, 15% Glass Fiber, Flame Retardant 15% Glass fiber reinforced, flame retardant PBT for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50mm/min; ISO 527-1/-2 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing 10% Glass Fiber. |