Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D638 |
SABIC 324CN Linear Low Density Polyethylene for Wire & Cable Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ISO 527 |
Polimeri Europa Riblene® GM 30 R Low Density Polyethylene - Coating Grade Riblene GM 30 R is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 R is suitable for coating applications where low neck-in and high manufacturing speed are.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D412 |
Precision Polymer Engineering V90D Fluoroelastomer Compound Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
across flow; ASTM D412 |
ExxonMobil Santoprene® 8203-45 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic general purpose non-hygroscopic elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ISO 527 |
Polimeri Europa Flexirene® MS 40 A Linear Low Density Polyethylene Flexirene MS 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 40 A are characterized by a good balance be.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | 500 mm/min (20 in./min.); Type IV Specimen; ASTM D638 |
Eastman 18DOA Polyethylene
(discontinued **) Polyethylene 18DOA is a low density formulation suggested for the production of closures where a high melt index material is needed to meet shrinkage requirements and fast molding cycles. It molds .. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | |
LyondellBasell Lupolen® 2420 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | |
LyondellBasell Lupolen® 2425 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | |
LyondellBasell Lupolen® 2426 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex APEX® 90-A472R-65-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | 2"/min; ASTM D638 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | 2"/min; ASTM D638 |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | 2"/min; ASTM D638 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | |
Trelleborg E645 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | >= 11.0 MPa | >= 1600 psi | |
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | Cable - At 2 inch/min; ASTM D638 |
Borealis Casico™ FR4804 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Borstar FR4804 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion p.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D-638 |
Axiall 8642 Moldings & Extrusions Flexible PVC General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Tensile Strength, Yield | 11.0 - 22.0 MPa | 1600 - 3190 psi | Average value: 18.1 MPa Grade Count:66 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |