Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 765 MPa @Strain 0.200 %, Temperature 650 °C |
111000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 25 alloy, cold worked sheet, 15 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 %, Temperature 371 °C |
111000 psi @Strain 0.200 %, Temperature 700 °F |
|
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 %, Thickness 50.8 mm |
111000 psi @Strain 0.200 %, Thickness 2.00 in |
|
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |