Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527-1 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min |
Arkema Group Oroglas® MI-2T Acrylic
(discontinued **) OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527 type 1 A |
Solvay TECHNYL® C 507XT PA6, DRY Description: Unreinforced polyamide 6, heat stabilized, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rod.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DFB03GR PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DFB03GR is a compound based on Polycarbonate resin containing a mixture of Glass Fiber and Glass Beads. Added features of this material include: Easy Molding. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527-1/-2 |
Unitika A1030BRL PA6, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527-1/-2 |
Unitika A1030FR PA6, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | GB/1040 |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527-1/-2 |
Covestro Apec® DP1-9389/5 Polycarbonate Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | |
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50mm/min; ISO 527 |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50mm/min; ISO 527 |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min |
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |
|||
Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO R527 |
Arkema Group Orgalloy® RS 6015 ES T6L Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |