Mechanical Properties Metric English Comments
Tensile Strength, Yield 930 - 1210 MPa
135000 - 175000 psi
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17000)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Yield 890 - 1210 MPa
129000 - 175000 psi
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; AT (TF00) Temper (UNS C17200)
Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 890 - 1210 MPa
129000 - 175000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17200)
Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 890 - 1210 MPa
129000 - 175000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17200)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 960 - 1210 MPa
139000 - 175000 psi
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200)
Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Tensile Strength, Yield 890 - 1210 MPa
129000 - 175000 psi
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; over 76 mm o.d. (UNS C17200)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 990 - 1210 MPa
144000 - 175000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 1060 - 1210 MPa
154000 - 175000 psi
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 990 - 1210 MPa
144000 - 175000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17200)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 990 - 1210 MPa
144000 - 175000 psi
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; up to 76 mm o.d. (UNS C17200)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 890 - 1210 MPa
129000 - 175000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17300)
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 862 - 1210 MPa

@Strain 0.200 %
125000 - 175000 psi

@Strain 0.200 %
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ..