Polymer Property : Tensile Strength, Yield = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 - 90.0 MPa
11600 - 13100 psi
Injection; ISO 527
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Tensile Strength, Yield 80.0 - 90.0 MPa
11600 - 13100 psi
Injection; ISO 527
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Tensile Strength, Yield 50.0 - 90.0 MPa
7250 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Tensile Strength, Yield 50.0 - 90.0 MPa
7250 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Tensile Strength, Yield 60.0 - 90.0 MPa
8700 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Tensile Strength, Yield 70.0 - 90.0 MPa
10200 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Tensile Strength, Yield 50.0 - 90.0 MPa
7250 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Tensile Strength, Yield 60.0 - 90.0 MPa

@Thickness 4.00 mm,
Temperature 23.0 °C
8700 - 13100 psi

@Thickness 0.157 in,
Temperature 73.4 °F
depending on color; ISO 527-2/5
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Strength, Yield 13.0 - 90.0 MPa
1890 - 13100 psi
Average value: 66.5 MPa Grade Count:109
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Tensile Strength, Yield 29.0 - 90.3 MPa
4210 - 13100 psi
Average value: 64.1 MPa Grade Count:18
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Tensile Strength, Yield 20.0 - 90.0 MPa

@Temperature -40.0 - 120 °C
2900 - 13100 psi

@Temperature -40.0 - 248 °F
Average value: 45.0 MPa Grade Count:1
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Yield 25.0 - 90.0 MPa
3630 - 13100 psi
Average value: 63.5 MPa Grade Count:41
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Tensile Strength, Yield 82.0 - 90.0 MPa
11900 - 13100 psi
Average value: 88.0 MPa Grade Count:5
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Tensile Strength, Yield 35.0 - 90.0 MPa
5080 - 13100 psi
Average value: 65.7 MPa Grade Count:54
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Tensile Strength, Yield 43.4 - 90.3 MPa
6300 - 13100 psi
Average value: 75.3 MPa Grade Count:22
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Tensile Strength, Yield 40.0 - 90.0 MPa
5800 - 13100 psi
Average value: 61.0 MPa Grade Count:10
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Yield 47.0 - 90.0 MPa
6820 - 13100 psi
Average value: 62.4 MPa Grade Count:26
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Tensile Strength, Yield 25.0 - 90.0 MPa
3630 - 13100 psi
Average value: 59.6 MPa Grade Count:99
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..