Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.30 MPa | 1350 psi | -25% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated .. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | 510 mm/min; ASTM D412A |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength, Yield | >= 9.30 MPa | >= 1350 psi | |
Kazanorgsintez 10803-020 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Tensile Strength, Yield | >= 9.32 MPa | >= 1350 psi | |
Kazanorgsintez 11503-070 UUP Low Density Polyethylene Production Method: LDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Designed for packaging and production of products designed for food contact, toy p.. |
|||
Tensile Strength, Yield | >= 9.30 MPa | >= 1350 psi | |
Kazanorgsintez 15813-020 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | 200 mm/min; ASTM D638 |
LG Chemical LUTENE LB4500 LDPE Extrusion Coating Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silico.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | ASTM D638 |
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous.. |
|||
Tensile Strength, Yield | 9.30 MPa | 1350 psi | |
Kraton® D1102 + LDPE blend (10/90) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 8103 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive Interior PartsInformation .. |
|||
Tensile Strength, Yield | >= 9.31 MPa | >= 1350 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7182E Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D412 |
Teknor Apex APEX® 3211-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S190A Thermoplastic Polyurethane Type: Estane® S190A is a Shore 92A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® CR185A Thermoplastic Polyurethane Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 9.30 MPa | 1350 psi | ASTM D638 |
Diamond Polymers NPP10-2528 Ethylene Vinyl Acetate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 300 % |
1350 psi @Strain 300 % |
ASTM D412 |
Dow SE BR-1203H Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1203H is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 300 % |
1350 psi @Strain 300 % |
ASTM D412 |
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1220M is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 6704 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 50.0 % |
1350 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 10706 Wire & Cable Flexible PVC Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 4750 Flexible PVC General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-5145D Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo.. |
|||
Tensile Strength, Yield | >= 9.30 MPa | >= 1350 psi | |
Kazanorgsintez 11503-070 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |