Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 950 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
Typical, Longitudinal Direction
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel
Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially ..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
Typical, Longitudinal Direction
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability
Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %,
Temperature 95.0 °C
138000 psi

@Strain 0.200 %,
Temperature 203 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %,
Temperature 550 °C
138000 psi

@Strain 0.200 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
Tensile Strength, Yield 950 - 1250 MPa

@Strain 0.200 %
138000 - 181000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1200 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..
Tensile Strength, Yield 950 MPa
138000 psi
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 950 MPa
138000 psi
ThyssenKrupp SECURE 400 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.App..
Tensile Strength, Yield 950 MPa
138000 psi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2
Information provided by HexCel
Tensile Strength, Yield >= 950 MPa

@Strain 0.200 %
>= 138000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield 951 MPa
138000 psi
Hardened 1900°F, Tempered 1000°F
ATI Allegheny Ludlum 420 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Yield 952 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Tensile Strength, Yield 950 - 1200 MPa
138000 - 174000 psi
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..
Tensile Strength, Yield 951 MPa

@Strain 0.200 %,
Temperature 316 °C
138000 psi

@Strain 0.200 %,
Temperature 601 °F
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 951 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper
Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles..
Tensile Strength, Yield 952 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC
Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t..