Polymer Property : Tensile Strength, Yield = 14.766 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.766 MPa
2141.6 psi
7% change after 70 hours @ 150°C; ASTM D412
Precision Polymer Engineering P70B Polyacrylate Rubber
Polyacrylic or Polyacrylate Rubber, 65-75 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi..