Polymer Property : Tensile Strength, Yield = 15000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.1 - 103 MPa
6260 - 15000 psi
Average value: 75.1 MPa Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Tensile Strength, Yield 34.5 - 103 MPa
5000 - 15000 psi
0.2% offset
Eagle Brass 210 Gilding Metal, Annealed
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Yield 30.0 - 103 MPa
4350 - 15000 psi
Average value: 56.9 MPa Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Tensile Strength, Yield 0.241 - 103 MPa
35.0 - 15000 psi
Average value: 30.3 MPa Grade Count:43
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..