Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM Data |
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Yield | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Tensile Strength, Yield | 105 - 234 MPa | 15200 - 34000 psi | Average value: 180 MPa Grade Count:55 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010M PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010P PEI Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 4002 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | |
Alcoa MIC-6 Aluminum Mold Alloy MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of i.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
Polyram PlusTek PB300G2 Nylon 6 for Injection Molding, 10% Glass-Fiber Reinforced 10% Glass-fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO R527 Type 1 |
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix HexPly® 6376 is a high performance tough matrix formulated for the fabrication of primary aircraft structures. It offers high impact resistance and damage tolerance for a wide range of high tempera.. |
|||
Tensile Strength, Yield | >= 105 MPa @Strain 0.200 % |
>= 15200 psi @Strain 0.200 % |
|
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50mm/min; ISO 527-1/-2 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |