Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 172 MPa | 25000 psi | |
Pacific Sintered Materials F-241-T Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-20All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | |
PSM Industries Pacific Sintered Metals Nickel Iron FN-250-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0200-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | .01% permanent set |
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | .01% permanent set |
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM L NAT002 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | Annealed |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessin.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 RM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Low Moisture Absorption and.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific) LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Strength, Yield | >= 172 MPa | >= 25000 psi | 0.2% Offset |
Eagle Brass 305 Austenitic Stainless Steel, Annealed Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Tensile Strength, Yield | >= 172 MPa | >= 25000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, Annealed Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | 172 - 476 MPa | 25000 - 69000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Yield | 172 - 455 MPa | 25000 - 66000 psi | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Tensile Strength, Yield | 172 - 365 MPa | 25000 - 53000 psi | |
Chicago Extruded Metals UNS C48200 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 172 - 365 MPa | 25000 - 53000 psi | |
Chicago Extruded Metals UNS C48500 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 172 MPa @Strain 0.200 %, Temperature 649 °C |
24900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Asahi Kasei Thermylon® NSG-730A 65% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |