Polymer Property : Tensile Strength, Yield = 188000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1296 MPa

@Strain 0.200 %
188000 psi

@Strain 0.200 %
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 1296 MPa

@Strain 0.200 %,
Temperature 316 °C
188000 psi

@Strain 0.200 %,
Temperature 601 °F
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..