Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek C81500 Chrome Copper High Conductivity Information provided by MetalTekCast UNS C81500; Cast Grade C81500; Military MIL-C-19310 |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 20-10 Cast UNS J92603 Heat Resistant Stainless Steel Economical heat resistant grade with sufficient chrome and nickel for good oxidation resistance.Applications: Burner tips, furnace rails, annealing boxes, trays, burnishing rolls.Information provide.. |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 25-12 Cast UNS J93503 Heat Resistant Stainless Steel Very sensitive to composition balance. Suitable for a wide range of high temperature applications.Applications: Rable arms, radiant tubes, refractory support hardware, grate bars.Information provide.. |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 317 Cast UNS J93000 Austenitic Stainless Steel "300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 317L Cast UNS J92999 Austenitic Stainless Steel "300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 25-20 Cast UNS J94224 Heat Resistant Stainless Steel Increased strength for more highly stressed applications. Good resistance to oxidizing or reducing process flow.Applications: Calcining tubes, pier caps, high temperature fixtures and hardware.Infor.. |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 25-35Nb Heat Resistant Stainless Steel Information provided by MetalTekCast ASTM A297 MOD. |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 27-5 Cast UNS J93015 Heat Resistant Stainless Steel Higher nickel yields improved strength. Resists high sulfur process gas.Applications: Pour spouts, holding pots, kiln parts, gas parts.Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 28-48WCo Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | |
MetalTek MTEK 30-20 Cast UNS N08604 Heat Resistant Stainless Steel Provides strength levels of HK with improved corrosion resistance to hot gases.Applications: Similar to HN.Information provided by MetalTekCast UNS N08604; Cast Grade HL; Cast ASTM A297, A608 |
|||
Tensile Strength, Yield | 240 MPa | 34800 psi | Annealed |
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |
|||
Tensile Strength, Yield | 240 MPa @Strain 0.200 % |
34800 psi @Strain 0.200 % |
Annealed |
Special Metals MONEL® Alloy R-405 The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a.. |
|||
Tensile Strength, Yield | >= 240 MPa @Strain 0.200 % |
>= 34800 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® DC02 (Fe P03) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Tensile Strength, Yield | 240 MPa | 34800 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Tensile Strength, Yield | 240 MPa | 34800 psi | |
AK Steel Hot Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 240 MPa | >= 34800 psi | ASTM A240 |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726) Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless.. |
|||
Tensile Strength, Yield | 240 MPa | 34800 psi | As Cast |
AFE Technologies Cronite 37Ni/18Cr No. HR5 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Tensile Strength, Yield | >= 240 MPa @Strain 0.200 % |
>= 34800 psi @Strain 0.200 % |
|
ALIMEX 2017A T451 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged. |
|||
Tensile Strength, Yield | >= 240 MPa @Strain 0.200 % |
>= 34800 psi @Strain 0.200 % |
|
ALIMEX 6082 T651 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged. |
|||
Tensile Strength, Yield | 240 MPa @Temperature 870 °C |
34800 psi @Temperature 1600 °F |
|
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |